Elantas PDG Pedigree® Two-Component, Flexible Low Odor Polyester Resin, Room Temperature Cure Type, 350 V/Mil (As Made), 250 V/Mil (After 24 hr in Water (ASTM D149)) Dielectric Strength, 66% Elongation, 88 °F (ASTM D93) Flash Point, 35 - 50 min At 25 °C (150 g) Gel Time, 30 Shore A Hardness, 100 (Parts By Weight) Mixing Ratio, 22 lb/Sq Inch Tensile Strength, 100 - 200 CP At 20 rpm 25 °C (77 °F) (ASTM D2196) Viscosity. - The Pedigree 300 LV is a two-component room temperature curing resin system. Its flexibility makes it an excellent choice for potting.
$14.83 / US pound
Min Qty:1
|Qty Increment:1
more info
more info
Elantas PDG Pedigree® Two-Component, Flexible Low Odor Polyester Resin, Room Temperature Cure Type, 350 V/Mil (As Made), 250 V/Mil (After 24 hr in Water (ASTM D149)) Dielectric Strength, 66% Elongation, 88 °F (ASTM D93) Flash Point, 35 - 50 min At 25 °C (150 g) Gel Time, 30 Shore A Hardness, 100 (Parts By Weight) Mixing Ratio, 22 lb/Sq Inch Tensile Strength, 100 - 200 CP At 20 rpm 25 °C (77 °F) (ASTM D2196) Viscosity. - The Pedigree 300 LV is a two-component room temperature curing resin system. Its flexibility makes it an excellent choice for potting.
- Attributes
- Features
- Applications
- Documents
Attributes
General Information
Item NameLow Odor Polyester Resin
Trade NamePedigree®
SeriesPedigree® PDG300LV5GL
General Features
Shelf Life3 Months
TypeTwo-Component, Flexible
Design & Construction
Cure TypeRoom Temperature
Performance Details
Tensile Strength22 lb/sq-Inch
Gel Time35 min
Technical Details
Flash Point88 °F
Chemical Properties
Mixing Ratio100 (Parts By Weight)
Viscosity100 cP
Electrical Properties
Dielectric Strength350 V/mil
Physical Properties
Container Size42 lb
Container TypePail
Hardness30 Shore A
Elongation66%
Features
- Flexible
- Can be highly filled for enhanced thermal conductivity
- Vacuum potting application methods
- This resin and hardener must be stored between at 25 °C in a dry controlled environment out of direct sunlight
- -5 °C glass transition temperature
- 200 ppm/°C coefficient of thermal expansion
- 85 Mil film thickness
- 0.03 at 25 °C (77 °F), 1 kHz (ASTM D150) dissipation factor
- 5.4 at 25 °C (77 °F), 1 kHz (ASTM D150) dielectric constant
- Container Size: 42 lb/5 gal
- Dielectric Strength: 350 V/Mil (As Made), 250 V/Mil (After 24 hr in Water (ASTM D149))
- Flash Point: 88 °F (ASTM D93)
- Viscosity: 100 - 200 CP at 20 rpm 25 °C/77 °F/ASTM D2196)
- Gel Time: 35 - 50 min
- Viscosity: 100 - 200 cP
Applications
- Potting and Sealing of Electrical and Electronic Equipment
- Electromagnetic Devices
- Low Voltage Transformers
- Chokes
- Toroids
- Ballast Insulation
- Power Supplies
- Lifting Magnets